Nanoindenters - Nanohardness tester

Today's nanoindenters offer more than nanoindentation. They allow further nano- and micro-tribological measurement methods like for example scratch tests and are universal platforms for complex, ... more 

Today's nanoindenters offer more than nanoindentation. They allow further nano- and micro-tribological measurement methods like for example scratch tests and are universal platforms for complex, mechanical material characterizations.

Nanoindentation, or depth-sensing hardness testing, is a method to mechanically characterize the micro structures of materials and to analyze thin films.

The Nanohardness Tester NanoTest offers other unique tribological measurement options: a patented nano-impact test which works like a nano-mechanical charpy test, nano fretting tests for high-cycle wear tests, and more.

NanoTest is the unparalleled testing platform for the nano and micro mechanical characterization of all sorts of materials: From metals and alloys over ceramics and polymers all the way to thin and ultra-thin films.

Properties that can be measured:

  • Nanohardness
  • Elastic modulus
  • 3D-Mapping of mechanical properties
  • Creep, elastic recovery and plasticity index
  • Dynamic nanohardness
  • Coefficient of friction and adhesion
  • High and low cycle fatigue
16. December 2019  - 17. December 2019 : National Centre for Advanced Tribology at the University of Southampton on the south coast of England.

Micro Materials Annual Conference and User Workshop

European visitors can reach Southampton fairly easily by train from the London airports – and the airline Flybe also operates direct routes to Southampton airport from some European cities – see ...
Nanoindenters - Nanohardness tester - Short introduction: nanoindentation
Short introduction: nanoindentation

Instrumented indentation tests, commonly known as nanoindentation, allow the precise application of a defined force of an indenter tip while simultaneously measuring the indentation depth into the ...


Nanoindenters - Nanohardness tester - Nanoindenter
Nanoindenter

The nanoindenter NanoTest Vantage is a comprehensive nanomechanical testing platform which provides a variety of different techniques such as nanoindentation/nanohardness testing as well as ...


Nanoindenters - Nanohardness tester - Vacuum nanoindenter
Vacuum nanoindenter

The nanoindenter NanoText Xtreme is the first commercially available vacuum-nanoindenter with a unique temperature range, intended to measure at the forefront of high temperature nanoindentation for ...

Contact

Quantum Design GmbH

Roddarestigen 3
SE 182 35 Danderyd
Sweden

Phone:+46 8 41071791
E-mail:nordic@qd-europe.com
Cookie notice Cookies help us in providing our services. By using our services, you agree to the use of cookies. Privacy policy